Here is the elemental information on the CK-4 series.
To answer the questions in advance the aluminum content comes with the high concentration of Molybdenum. It is part of that raw material. The 7 ppm Silicon is defoamer.
Here is the elemental information on the CK-4 series.
To answer the questions in advance the aluminum content comes with the high concentration of Molybdenum. It is part of that raw material. The 7 ppm Silicon is defoamer.
Does anybody know the ash content of these oils outa curiosity?
I was debating for awhile on the next oil to try in my 6.7 Powerstroke, and after chatting with Dave, the super fast and helpful response was enough for me to give HPL a try, just received this week, looking forward to getting it in there. Was undecided on trying a 10w30 of sorts, but decided to go with another 5w-40 in HPL.