The VOA of the SAE 40 is ready.
Nothing really jumps out other than the trace aluminum that was mentioned earlier that is residue from the catalyst. The Mg/Ca ratio and levels are essentially identical to the 15w-40, as are Zn and P levels. The 10ppm silicon from the antifoam package is pretty typical of the HPL PCMOs.
Perhaps the virgin oxidation is slightly higher as a result of the extra esters used to thicken the GTL up a bit. I think that in general the heavier grade PCMO line gets more AN and less ester so they seem to run lower on virgin oxidation vs the low 30s...
Nothing really jumps out other than the trace aluminum that was mentioned earlier that is residue from the catalyst. The Mg/Ca ratio and levels are essentially identical to the 15w-40, as are Zn and P levels. The 10ppm silicon from the antifoam package is pretty typical of the HPL PCMOs.
Perhaps the virgin oxidation is slightly higher as a result of the extra esters used to thicken the GTL up a bit. I think that in general the heavier grade PCMO line gets more AN and less ester so they seem to run lower on virgin oxidation vs the low 30s...